China's earliest production and processing of aluminum veneer ceiling, one of the curtain wall manufacturers
aluminum honeycomb panelIn the process of making the panel and the back plate, the edge of the plate needs to be folded up. The folding machine used in the traditional process will form stress in the metal because of one-time rapid folding, and will form micro damage to the metal, affecting the service life of the metal. The rolling forming technology uses ten rollers to gradually fold the edge of the plate to a preset angle, gradually forming to ensure the release of internal stress, and the damage to the metal itself is reduced to a minimum.
continuous pre-roll coating technology
When the aluminum coil is formed, the coating color is attached to the above technology, the coating adhesion is strong, the durability is good, the color is uniform, and the Products of the same batch basically do not have any color difference.
技术数据:密度(kg/㎡) 3.6~5.3
Unflatness <0.2mm
Boards thermal resistance 0.026 m2.k/w
Equivalent thermal conductivity 0.88w/m.k
Sound insulation 29dB
弹性模量 4×104MN/㎡
弯曲抗拉强度 ≥83MN/㎡
抗剪强度 2MN/㎡
刚度(kN.㎡) 1.0~23.0
防火等级 B1级(GIN)
Recommended article:
Main features of aluminum honeycomb board
/Article/lvfengwobanbandezhuy_1.html
Single Material and Structure of Aluminum Honeycomb Plate
/Article/lvfengwobandancaizhi_1.html
What is wood grain aluminum veneer
/Article/shimeshimuwenlvdanba_1.html